Quartz imitation stone bricks have a hard texture and can withstand wind and rain. They have been used in various places now. With the continuous development of technology, creative ceramic tiles have catered to everyone's home decoration concepts. Do you know what problems may arise during the production process of quartz imitation stone bricks in Shandong? The following is an introduction from the manufacturer:
1、破碎:是指將石英仿石磚破碎成一定比例的顆粒,但破碎顆粒的大小和比例會影響其透水性、表面效應、強度、半成品尺寸和燒成溫度,顆粒越粗,透水性越好,但坯體強度會降低,表面效果粗糙,尺寸增大,燒成溫度升高。
1. Crushing: refers to breaking quartz imitation stone bricks into particles of a certain proportion, but the size and proportion of the broken particles will affect their water permeability, surface effect, strength, semi-finished product size, and firing temperature. The thicker the particles, the better their water permeability, but the strength of the body will decrease, the surface effect is coarse, the size increases, and the firing temperature increases.
2、在混合攪拌過程中,加入一定量的熔劑和粘結劑,提高生坯的強度和球團之間的附著力,如果不加就不能成型,或者強度不夠,半成品損耗大,成品石英仿石磚有很多裂紋。
2. During the mixing and stirring process, a certain amount of flux and adhesive is added to improve the strength of the green body and the adhesion between the pellets. If it is not added, it cannot be formed, or the strength is insufficient, resulting in large loss of semi-finished products, and many cracks in the finished quartz imitation stone brick.
3、如果成形壓力機是自動壓力機,它需要一個輔助分配系統,石英仿石磚通常由織物和基材組成,織物與基材的比例約為1:6,對于仿磚的成型,在降低設備投資、設備維護成本和使用廉價勞動力的同時,很多企業會采用摩擦壓磚機或振動壓磚機來滿足工藝要求。
3. If the forming press is an automatic press, it requires an auxiliary distribution system. Quartz imitation stone bricks are usually composed of fabric and substrate, with a ratio of about 1:6. For the formation of imitation bricks, while reducing equipment investment, equipment maintenance costs, and using cheap labor, many enterprises will use friction or vibration presses to meet process requirements.
4、窯燒通常用于燒制石英仿石磚,其厚度約為60毫米,燒制時間約為20小時,同時,棚車大約有八層,燒成溫度為1200-1250攝氏度。
4. Kiln firing is commonly used to fire quartz imitation stone bricks, which have a thickness of about 60 millimeters and a firing time of about 20 hours. At the same time, the box car has about eight layers and a firing temperature of 1200-1250 degrees Celsius.